- ADASTHERM® DB(DMD B:DACRON+FILM +DACRON)
- ADASTHERM® DF(DMD F:DACRON+FILM +DACRON)
- ADASTHERM® NF(NMN:NOMEX+FILM +NOMEX)
- ADASTHERM® NH(NHN:NOMEX+POLIMIDE +NOMEX)
- ADASTHERM® AF(AMA:ARAMID+FILM +ARAMID)
- ADASTHERM® PREPREG
- ADASTHERM® FILM
- ADASTHERM® DDP(DIAMOND DOTTED PAPER)
- ADASTHERM® PE(PRESS PAPER +FILM )
- ADASTHERM® PAPER
- ADASTHERM® BOARD
- ADASTHERM® PMP
- POLYMIDE ADHESIVE TAPE
- CREPE PAPER
- PVC FIBERGLASS SLEEVING
- SILICONE FIBERGLASS SLEEVING
- ACRYLIC FIBERGLASS SLEEVING
- SILICONE RUBBER FIBERGLASS SLEEVING
- EXPANDABLE FIBERGLASS SLEEVING
- POLYURETHANE FIBERGLASS SLEEVING
- HTG FIBERGLASS SLEEVING
- FIRE SLEEVING
- PHENOLIC COTTON CLOTH LAMINATED SHEET
- PHENOLIC PAPER LAMINATED SHEET
- EPOXY PHENOLIC GLASS CLOTH LAMINATED SHEET
- FR-4 G10 G11
- PHENOLIC COTTON CLOTH LAMINATED ROD
- EPOXY PHENOLIC GLASS CLOTH LAMINATED ROD
Specifications: The thickness of base paper is from 0.05-0.075-0.08-0.13, and the thickness after wrinkling is 027-0.35-0.46-0.55-0.8.
NO. |
Test Conditions |
Temperature 22.0℃ |
Relative humidity |
40.0%r.h |
|||
1 |
Metric name: |
Unit: |
Index: |
Actual data: |
Test method: |
||
2 |
Thickness |
mm |
0.05±0.05 |
0.053 |
GB/T451.3 |
||
3 |
Fix quantify |
g/㎡ |
65±10% |
68 |
GB/T451.2 |
||
4 |
Ash content≤ |
% |
0.7 |
0.68 |
GB/T742 |
||
5 |
Moisture≤ |
% |
6 |
5.9 |
GB/T462 |
||
6 |
PH of water extract |
|
6.5~8 |
7 |
GB/T1545.2 |
||
7 |
Tensile strength≥ |
Horizontal |
KN/M |
1.6 |
1.58 |
GB/T453 |
|
portrait |
3.5 |
3.8 |
|||||
8 |
Elongation at break wrinkle |
% |
50±10% |
45 |
GB/T453 |
||
9 |
Dry paper loss(tg&)(100℃)not less than |
% |
|
0.16 |
GB/T3334 |
||
10 |
Power frequency breakdown voltage after stretching and leveling a layer of invading transformer oil≥ |
KV |
2.2 |
2.2 |
GB/T3333 |
||
11 |
Power frequency breakdown voltage in air≥ |
V |
800 |
900 |
GB/T3333 |